| Technical Measurement | Performance |
|---|---|
| Coating Element | Iridium Oxide (IrO₂), Tantalum Oxide (Ta₂O₅) |
| Coating Thickness | 6~12 μm |
| Coating Uniformity | 85% min. |
| Technical Measurement | Performance |
|---|---|
| Current Density | 500~800 A/m² |
| Operating Voltage | ≤ 24V |
| pH Range | 1~14 |
| Temperature | < 85 °C |